The troublesome & fragile FF/Rew linkage of a wm-1, patched up for duplication & conversion to metal





Duplicate in dental acrylic out of the mould ready to go tp the dental lab (my technician knows I am eccentric) for casting into metal (spruing/investing/burnout/casting with Nickel Chrome alloy)





But then oooops...what about the spring...Lucky for us we have Orthodontic stainless steel wire :lol:











Transplanted artificial replacement in place Operation a success :-D
 